For the evaluation of the accelerated degradation in laboratory of red ceramic specimens with addition of ornamental rock waste free from steel particles, an equipment that leach with hot and cool water and time control, and also freezing the specimen at -4 ºC was used,. The ceramic samples were made with up to 10 wt.% of the dry ornamental rock waste, and after humidifying and molding by extrusion. The specimens were fired at 700 ºC, 800 ºC and 900 ºC. After 1060 h of accelerated degradation lab test, ceramic properties were evaluated. The results of the strength were compared for Weibull distribution, before and after degradation. The specimens with addition of 10 wt.% waste is more durable and reliable when fired to 900 ºC after the degradation.
red ceramic; ornamental rock waste; durability; Weibull distribution