Poly(3-octylthiophene)/stearic Acid Langmuir and Langmuir-Blodgett films: Preparation and characterization

A study is reported on Langmuir and Langmuir-Blodgett (LB) films obtained by adding different percentages of stearic acid (SA) to poly(3-octylhiophene) (P3OT). Surface pressure - mean molecular area (π - A) isotherms, ultraviolet-visible (UV-Vis) absorption spectrum, atomic force microscope (AFM) and dc electrical measurements have been used for characterization. From π - A isotherms, the area per monomer for condensed films (of SA) increased according to P3OT amount. Good transfer ratios were obtained for LB deposition from P3OT/SA films with higher percentage of SA. LB films revealed linear growth as monitored by UV-Vis absorption spectra. Electrical characterization showed higher conductivity for LB film with 54 wt.% of SA. AFM images of the same film revealed high roughness and presence of large size agglomerates. Finally, interdigitated electrodes (IDE) coated with P3OT/SA LB films showed to be sensitive to the presence of volatile organic compounds.

Langmuir; Langmuir-Blodgett; polythiophenes; electrical characterization; sensors


ABM, ABC, ABPol UFSCar - Dep. de Engenharia de Materiais, Rod. Washington Luiz, km 235, 13565-905 - São Carlos - SP- Brasil. Tel (55 16) 3351-9487 - São Carlos - SP - Brazil
E-mail: pessan@ufscar.br