PURPOSE: To evaluate the effect of the use of 0.5% and 2% chlorhexidine digluconate on the immediate bond strength of a conventional adhesive system to dentin in primary teeth. METHODS: Twenty-one healthy primary molars were divided into three groups (n=7), being one control (A) and two experimental groups (B and C). After dentin exposure, in Group (A) the adhesive procedure was performed using 37% phosphoric acid gel (15 s); dentin was washed (15 s), air dried (30 s) and rehydrated with water. Groups B and C followed similar procedures but for re-hydration with 0.5% and 2% chlorhexidine, respectively, for 30 s. A resin composite block was built simulating a restoration, and the teeth were stored in distilled water at 37°C for 24 h before the microtensile bond strength test. The bond strength data were analyzed by analysis of variance. RESULTS: No statistically significant difference in bond strength was found among the tested groups (P>0.05) CONCLUSION: The 0.5% and 2% concentrations of chlorhexidine presented similar behavior and caused no adverse effects on the bond strength to dentin in primary teeth.
Chlorhexidine; bond strength; microtensile; primary teeth