Synthesis and catalytic properties of iron - cerium phosphates with surfactant

Síntese e propriedades catalíticas de ferro-fosfato de cério com surfactante

Iron phosphate was prepared from iron nitrate and phosphoric acid with a surfactant, pentaethylene glycol mono dodecyl ether. The chemical composition of the obtained samples was estimated from ICP and XRD measurements. Particle shape and size distribution were observed by SEM images and laser diffraction / scattering methods. Further, the catalytic activity was studied with the decomposition of the complex between formaldehyde, ammonium acetate, and acetylacetone. The peaks of FePO4 were observed in XRD patterns of samples prepared in Fe/Ce=10/0 and then heated at 600 ºC. Other samples were amorphous in XRD patterns. Iron-cerium phosphates had high catalytic activity for the decomposition of the complex.

iron phosphate; cerium substitution; surfactant; ICP analysis; catalytic property


Associação Brasileira de Cerâmica Av. Prof. Almeida Prado, 532 - IPT - Prédio 36 - 2º Andar - Sala 03 , Cidade Universitária - 05508-901 - São Paulo/SP -Brazil, Tel./Fax: +55 (11) 3768-7101 / +55 (11) 3768-4284 - São Paulo - SP - Brazil
E-mail: ceram.abc@gmail.com